1310nm band PANDA fiber Fujikura PANDA fibers have a superior optical property in polarization-maintaining because of the symmetrical accuracy in cross section and the uniform constitution of stress applying parts. Based on Fujikura's fiber technology, PANDA fibers have a universal quality with not only low polarization-crosstalk and low attenuation but also the broad suitability for fusion-splice or optical connector. Contact us here for inquiries. contact us Features Specifications Others Features 1310nm band polarization maintaining fiber Low loss and low polarization crosstalk RoHS compliant Specifications Common specifications Concentricity error ≤0.5µm Cladding diameter 125±1µm (Major diameter) Polarization crosstalk ≤-30dB/100m@1310nm Minimum bending radius 1% proof : R30mm*2% proof : R20mm Product list Product Mode fielddiameter Attenuation Cutoffwavelength Beat length Coatingstructure Coatingdiameter SM13-PS-H90D 9.0±0.5µm@1310nm ≤1.0dB/km@1310nm 1130-1270nm 2.5-4.0mm@1310nm UV curable acrylate /Polyester elastomer(Color : Black) 900±100µm SM13-PS-U40D UV curable acrylate 400±15µm SM13-PS-U25D 245±15µm HA13-PS-U25D 5.5±1.0µm@1310nm ≤2.0dB/km@1310nm 1000-1290nm 2.5mm@1310nm *1% proof test type is standard. 2% proof test type is available, and code '-H' is added at the end of the product name. (e.g. SM15-PS-U40D-H) Others Catalog [PDF177KB] Contact us here for inquiries. contact us