1310nm band PANDA fiber

Fujikura PANDA fibers have a superior optical property in polarization-maintaining because of the symmetrical accuracy in cross section and the uniform constitution of stress applying parts. Based on Fujikura's fiber technology, PANDA fibers have a universal quality with not only low polarization-crosstalk and low attenuation but also the broad suitability for fusion-splice or optical connector.
- Contact us here for inquiries.
- contact us
Features
- 1310nm band polarization maintaining fiber
- Low loss and low polarization crosstalk
- RoHS compliant
Specifications
Common specifications
Concentricity error | ≤0.5µm |
---|---|
Cladding diameter | 125±1µm (Major diameter) |
Polarization crosstalk | ≤-30dB/100m@1310nm |
Minimum bending radius | 1% proof : R30mm* 2% proof : R20mm |
Product list
Product | Mode field diameter |
Attenuation | Cutoff wavelength |
Beat length | Coating structure |
Coating diameter |
---|---|---|---|---|---|---|
SM13-PS-H90D | 9.0±0.5µm @1310nm |
≤1.0dB/km @1310nm |
1130-1270nm | 2.5-4.0mm @1310nm |
UV curable acrylate /Polyester elastomer (Color : Black) |
900±100µm |
SM13-PS-U40D | UV curable acrylate | 400±15µm | ||||
SM13-PS-U25D | 245±15µm | |||||
HA13-PS-U25D | 5.5±1.0µm @1310nm |
≤2.0dB/km @1310nm |
1000-1290nm | 2.5mm @1310nm |
*1% proof test type is standard. 2% proof test type is available, and code '-H' is added at the end of the product name. (e.g. SM15-PS-U40D-H)